Two Kilos per Cubic Metre: Getting Internal Curing SAP Into the Mix
SAP dose for internal curing concrete, why dry addition steals slump, how to disperse without fish eyes, and what the desorption curve must show at 93 percent RH.
SAP dose for internal curing concrete, why dry addition steals slump, how to disperse without fish eyes, and what the desorption curve must show at 93 percent RH.
Internal curing needs two numbers: pore-solution absorption and 20-25 kg of extra water per kg of powder. Skip the second and slump falls.